Material Notes:
Description: Kraton G1657 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 13% . It is supplied from North America in the physical form identified: Kraton G1657 MS - supplied as a dusted pelletKraton G1657 MO - supplied as a dusted pelletRegion: Asia Pacific, Europe, Japan, North America, and South AmericaUses: Kraton G1657 M is used as a modifier of bitumen or thermoplastics and in compound formulations. It may also find use as an ingredient in formulating adhesives, sealants and coatings.Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Medical; Packaging and Polymod; and Personal CareInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D4025
Volatiles <= 1.0 %
<= 1.0 %
KM 04
Viscosity 1200 - 1800 cP
1200 - 1800 cP
20% Toluene Solution at 25°C; BAM 922
Melt Flow 22 g/10 min

@Load 5.00 kg,
Temperature 230 °C
22 g/10 min

@Load 11.0 lb,
Temperature 446 °F
Ash 0.020 - 0.12 %
0.020 - 0.12 %
S, For G1657 MS, silica dusted; BAM 908
Mechanical Properties Metric English Comments
Hardness, Shore A 47

@Time 10.0 sec
47

@Time 0.00278 hour
Typical values on polymer compression molded at 300°F; ASTM D2240
Tensile Strength 23.4 MPa
3390 psi
Typical properties of film cast from toluene solution; ASTM D412
Elongation at Break 750 %
750 %
Typical properties of film cast from toluene solution.; ASTM D412
300% Modulus 0.00241 GPa
0.350 ksi
Typical properties of film cast from toluene solution; ASTM D412
Chemical Properties Metric English Comments
Diblock Content 30 %
30 %
Descriptive Properties Value Comments
Content Dust, O
0.45-0.75%, BAM 1029
Non-staining phenolic antioxidant
0.03-0.1%, KM 08
Polystyrene
12.3-14.3%, Measured on the polymer before hydrogenation, KM 03
Total Extractables
<1.5%, KM 05
Styrene/Rubber Ratio 13/87