Material Notes:
Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A-B]n). The KRATON G series are second generation block polymers in which the rubber monomer is a saturated olefin polymer, either ethylene/butylene or ethylene/propylene. Kraton G polymer grades manufactured in France are labeled with an "E" for standard grades and "ES" for grades dusted with silica, for distribution in Europe, Africa and Asia Pacific. Information provided by the manufacturer, Kraton® Polymers.
Physical Properties Metric English Comments
Melt Flow 20.2 g/10 min
20.2 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.4 MPa
3390 psi
Elongation at Break 190 %
190 %
Flexural Modulus 2.10 GPa
305 ksi
Izod Impact, Notched 1.07 J/cm

@Temperature -30.0 °C
2.00 ft-lb/in

@Temperature -22.0 °F
3.2 mm (0.125 in) notch
8.00 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
3.2 mm (0.125 in) notch
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 78.8 °C
174 °F
Users viewing this material also viewed the following: