Material Notes:
Description: Kraton G1660 H is a linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 31%. It is supplied from North America in the physical form identified: G1660 HU - supplied as an undusted powder crumb.Region: Asia Pacific, Europe, Japan, North America, and South AmericaUses: Kraton G1660 H polymer is used as a modifier of thermoplastics and bitumen. It is also suitable as an ingredient in thermoplastic elastomer (TPE) compound formulations for a variety of applications and may be used in formulating adhesives, sealants, and coatings.Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Medical; Packaging and Polymod; and Personal CareInformation provided by Kraton®
Physical Properties Metric English Comments
Volatiles <= 1.0 %
<= 1.0 %
KM 04
Viscosity 900 - 1500 cP
900 - 1500 cP
20% Toluene Solution at 25°C; BAM 922
Descriptive Properties Value Comments
Content Polystyrene
29.2-32.6%, Measured on the polymer before hydrogenation, KM 03
Total Extractables
<1.0%, KM 05