Kraton® G2836 GT-N (SEBS) Compound

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Kraton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® G2836 GT-N (SEBS) Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton G2836 GT-N is a compound designed for film applications in the Personal Care market: Kraton G2836 GT-N - supplied as a dusted, dense pelletRegion: Asia Pacific, Europe, Japan, North America, and South AmericaApplications: Compounding and Personal Hygiene; and Personal CareInformation provided by Kraton®
Physical Properties Metric English Comments
Melt Flow 23 - 37 g/10 min

@Load 5.00 kg,
Temperature 230 °C
23 - 37 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 46 - 60
46 - 60
BAM 1003