Kuraray Genestarâ„¢ GW1458HF Nylon, 45% Glass Filled

Category Polymer , Thermoplastic , Nylon
Manufacturer Kuraray Company
Trade Name Genestar™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kuraray Genestarâ„¢ GW1458HF Nylon, 45% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low Warpage, High Flow HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
Water Absorption 1.1 %
1.1 %
Linear Mold Shrinkage, Flow 0.00050 cm/cm
0.00050 in/in
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
Melt Flow 90 g/10 min

@Load 2.16 kg,
Temperature 320 °C
90 g/10 min

@Load 4.76 lb,
Temperature 608 °F
ASTM D1238
Spiral Flow 6.20 cm

@Load 750 kg,
Temperature 320 °C
2.44 in

@Load 1650 lb,
Temperature 608 °F
0.5mm diameter
Mechanical Properties Metric English Comments
Tensile Strength 32.0 MPa
4640 psi
Weld; ASTM D638
150 MPa
21800 psi
ASTM D638
Elongation at Yield 0.40 %
0.40 %
Weld; ASTM D638
3.1 %
3.1 %
ASTM D638
Flexural Strength 207 MPa
30000 psi
ASTM D790
Flexural Modulus 13.0 GPa
1890 ksi
ASTM D790
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 306 °C
583 °F
Deflection Temperature at 1.8 MPa (264 psi) 290 °C
554 °F
ASTM D648
Glass Transition Temp, Tg 125 °C
257 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 30.0 kV/mm
762 kV/in
ASTM D149
Comparative Tracking Index >= 600 V
>= 600 V
ASTM UL746A