Kuraray Genestarâ„¢ N1006A-M41 Nylon

Category Polymer , Thermoplastic , Nylon
Manufacturer Kuraray Company
Trade Name Genestar™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kuraray Genestarâ„¢ N1006A-M41 Nylon.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact modified unreinforced injection grade. Main Features:High elongationHigh impact strengthExamples of applications are:Retainers for quick connectorFlexible band
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
Water Absorption 0.25 %
0.25 %
ISO 62
Linear Mold Shrinkage, Flow 0.014 cm/cm
0.014 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.015 cm/cm
0.015 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ISO 527-1/-2
Elongation at Break 20 %
20 %
ISO 527-1/-2
Elongation at Yield 7.0 %
7.0 %
ISO 527-1/-2
Tensile Modulus 1.88 GPa
273 ksi
ISO 527-1/-2
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Flexural Modulus 1.50 GPa
218 ksi
ISO 178
Charpy Impact, Notched 6.50 J/cm²
30.9 ft-lb/in²
ISO 179/1eA
Coefficient of Friction 0.25
0.25
ISO JIS K7218-A
K Factor (Wear Factor) 50
50
[mg]
Limiting Pressure Velocity 0.980 MPa-m/sec
28000 psi-ft/min
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
ASTM D696
CTE, linear, Transverse to Flow 67.0 µm/m-°C
37.2 µin/in-°F
ASTM D696
Melting Point 300 °C
572 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ISO 75-1/-2
Glass Transition Temp, Tg 125 °C
257 °F
10°C/min; ISO 11357-1/-2
Descriptive Properties Value Comments
Applications Automotive
General Purpose
Chemical Resistance Acid Resistance
Alkali Resistance
Environmental Stress Crack Resistance
General Chemical Resistance
Grease Resistance
Hydrolytically Stable
Oil Resistance
Solvent Resistance
Delivery Form Black
Natural Color
Other Features Barrier Properties
Creep Resistance
High Crystalinity
Thermal Stability
Weldable
Processing Injection Molding
Regional Availability Asia Pacific
Europe
Near East/Africa
North America
South and Central America
Special Characteristics Heat Stabilized or Stable to Heat
High Impact or Impact Modified