Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kuraray HYBRAR® A1 Thermoplastic Rubber-ABS Blend

Category Polymer , Thermoplastic , ABS Polymer , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Kuraray Company
Trade Name HYBRAR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kuraray HYBRAR® A1 Thermoplastic Rubber-ABS Blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber which exhibits high vibration damping properties at room temperatures. Both hydrogenated and non-hydrogenated grades of HYBRAR® are available. In addition to the superior vibration damping properties, hydrogenated grades also exhibit excellent miscibility with polypropylene, and may be used to produce blends with excellent transparency, flexibility and mechanical properties.Blends of HYBRAR® and other polymers exhibit excellent vibration damping properties.Mixing Conditions: Single Screw Extruder @ 210°CMolding Conditions: Injection molding, Cylinder @ 230°C, Mold @ 50°CFormulation (parts by weight): ABS - 60, HYBRAR® 5127 - 10, Mica - 30, Silane Coupling Agent - 0.16Information provided by The Kuraray Group.
Mechanical Properties Metric English Comments
Flexural Yield Strength 59.0 MPa
8560 psi
Izod Impact, Notched 0.290 J/cm
0.543 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 99.8 °C
212 °F
Pressure Not Specified
Descriptive Properties Value Comments
Tan Delta 0.032
at 40°C, measured w/ Rheovibron @ 11 Hz
0.035
at 25°C, measured w/ Rheovibron @ 11 Hz
0.053
at 10°C, measured w/ Rheovibron @ 11 Hz
0.077
at 0°C, measured w/ Rheovibron @ 11 Hz