Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LATI LASTANE 50 G/40 40% Glass Fiber Reinforced Polyurethane (PUR)  (discontinued **)

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI LASTANE 50 G/40 40% Glass Fiber Reinforced Polyurethane (PUR)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These properties make the Lastanes very suitable for wheels, gears, couplings, parts of textile machinery, shoes, and others. Reinforced Lastanes are used when good rigidity and high dimensional stability are required.Specific Notes for this Material: 40% glass fiber; very low molding shrinkage; good dimensional stability; good noise inertness; good rigidity; good impact resistance even at low temperatures.Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.All data provided by LATI.
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
Water Absorption 0.30 %
0.30 %
at 23°C; ISO 62
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
LATI
Linear Mold Shrinkage, Transverse 0.0020 cm/cm
0.0020 in/in
LATI
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 75.0 MPa
10900 psi
ISO 527
Flexural Modulus 2.30 GPa
334 ksi
ASTM D790
Izod Impact, Notched 6.00 J/cm
11.2 ft-lb/in
ASTM D256
2.00 J/cm

@Temperature -40.0 °C
3.75 ft-lb/in

@Temperature -40.0 °F
ASTM D256
4.00 J/cm

@Temperature -20.0 °C
7.49 ft-lb/in

@Temperature -4.00 °F
ASTM D256
Charpy Impact Unnotched >= 30.0 J/cm²
>= 143 ft-lb/in²
DIN 53453
6.50 J/cm²

@Temperature -40.0 °C
30.9 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
8.00 J/cm²

@Temperature -20.0 °C
38.1 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
Thermal Properties Metric English Comments
Vicat Softening Point 115 °C
239 °F
50°C/h 50N; ISO 306
Processing Properties Metric English Comments
Melt Temperature 200 - 220 °C
392 - 428 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Drying Temperature 80.0 - 100 °C
176 - 212 °F
Necessary, temperature can be reduced when using vacuum ovens.
Dry Time >= 3 hour
>= 3 hour
Necessary, drying time can be reduced when using vacuum ovens.
Descriptive Properties Value Comments
Injection Speed medium