LATI Latan 13 S/20 POM, 20% Glass Bead Reinforced

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Glass Bead Filled
Manufacturer LATI
Trade Name Latan
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latan 13 S/20 POM, 20% Glass Bead Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
Linear Mold Shrinkage, Flow 0.0185 - 0.0215 cm/cm
0.0185 - 0.0215 in/in
Linear Mold Shrinkage, Transverse 0.0185 - 0.021 cm/cm
0.0185 - 0.021 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa

@Temperature 60.0 °C
4350 psi

@Temperature 140 °F
45.0 MPa

@Temperature 23.0 °C
6530 psi

@Temperature 73.4 °F
Elongation at Break 15 %

@Temperature 23.0 °C
15 %

@Temperature 73.4 °F
70 %

@Temperature 60.0 °C
70 %

@Temperature 140 °F
>= 100 %

@Temperature 90.0 °C
>= 100 %

@Temperature 194 °F
Elongation at Yield 8.0 %

@Temperature 23.0 °C
8.0 %

@Temperature 73.4 °F
8.0 %

@Temperature 60.0 °C
8.0 %

@Temperature 140 °F
8.0 %

@Temperature 90.0 °C
8.0 %

@Temperature 194 °F
Tensile Modulus 1.20 GPa

@Temperature 90.0 °C
174 ksi

@Temperature 194 °F
2.00 GPa

@Temperature 60.0 °C
290 ksi

@Temperature 140 °F
3.10 GPa

@Temperature 23.0 °C
450 ksi

@Temperature 73.4 °F
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
239 °F
Vicat Softening Point 150 °C

@Load 5.00 kg
302 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V
A solution
Processing Properties Metric English Comments
Melt Temperature 180 - 210 °C
356 - 410 °F
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Drying Temperature 80.0 - 90.0 °C

@Time 10800 sec
176 - 194 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa
Copyright © lookpolymers.com All Rights Reserved