LATI Latigea B01 F1 Bio-Polymer

Category Polymer , Thermoplastic , Polylactic Acid (PLA) Biopolymer
Manufacturer LATI
Trade Name Latigea
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latigea B01 F1 Bio-Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bio-Polymer (PLA, PHB, ...). Unfilled. Potentially suitable for food/medical contact application. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
Linear Mold Shrinkage, Transverse 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.0 MPa
7980 psi
Elongation at Break 4.5 %
4.5 %
Elongation at Yield 2.8 %
2.8 %
Tensile Modulus 3.00 GPa
435 ksi
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
Charpy Impact, Notched 0.140 J/cm²
0.666 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 55.0 °C
131 °F
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
Vicat Softening Point 60.0 °C

@Load 5.00 kg
140 °F

@Load 11.0 lb
Processing Properties Metric English Comments
Melt Temperature 170 - 190 °C
338 - 374 °F
Mold Temperature 15.0 - 30.0 °C
59.0 - 86.0 °F
Drying Temperature 40.0 - 50.0 °C

@Time 21600 sec
104 - 122 °F

@Time 6.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa