Material Notes:
Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
Linear Mold Shrinkage, Transverse 0.0025 - 0.0065 cm/cm
0.0025 - 0.0065 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
Elongation at Break 9.0 %
9.0 %
Elongation at Yield 2.2 %
2.2 %
Tensile Modulus 2.90 GPa
421 ksi
Charpy Impact Unnotched 3.00 J/cm²
14.3 ft-lb/in²
Charpy Impact, Notched 0.380 J/cm²
1.81 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C
122 °F
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
Vicat Softening Point 55.0 °C

@Load 5.00 kg
131 °F

@Load 11.0 lb
Processing Properties Metric English Comments
Melt Temperature 170 - 190 °C
338 - 374 °F
Mold Temperature 15.0 - 30.0 °C
59.0 - 86.0 °F
Drying Temperature 40.0 - 50.0 °C

@Time 21600 sec
104 - 122 °F

@Time 6.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa