Material Notes:
Radiopaque compound based on Polypropylene copolymer (PPc). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
Linear Mold Shrinkage, Flow 0.014 - 0.018 cm/cm
0.014 - 0.018 in/in
Linear Mold Shrinkage, Transverse 0.014 - 0.018 cm/cm
0.014 - 0.018 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 5.00 MPa
725 psi
Elongation at Break >= 100 %
>= 100 %
Elongation at Yield >= 10 %
>= 10 %
Tensile Modulus 0.100 GPa
14.5 ksi
Charpy Impact Unnotched NB
NB
Charpy Impact, Notched NB
NB
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C
122 °F
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C
104 °F
Vicat Softening Point 60.0 °C

@Load 5.00 kg
140 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
Processing Properties Metric English Comments
Melt Temperature 200 - 240 °C
392 - 464 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Drying Temperature 80.0 - 90.0 °C

@Time 10800 sec
176 - 194 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa