LATI Latimass 82-05 D040 PA12

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer LATI
Trade Name Latimass
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latimass 82-05 D040 PA12.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 4.25 g/cc
0.154 lb/in³
Linear Mold Shrinkage, Flow 0.0035 - 0.0065 cm/cm
0.0035 - 0.0065 in/in
Linear Mold Shrinkage, Transverse 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.0 MPa
5080 psi
Elongation at Break 0.70 %
0.70 %
Tensile Modulus 4.50 GPa
653 ksi
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
Vicat Softening Point 165 °C

@Load 5.00 kg
329 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Volume Resistivity 6600 ohm-cm
6600 ohm-cm
Surface Resistance 5000 ohm
5000 ohm
Processing Properties Metric English Comments
Melt Temperature 250 - 270 °C
482 - 518 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 - 100 °C

@Time 10800 sec
176 - 212 °F

@Time 3.00 hour
Descriptive Properties Value Comments
Electromagnetic reflection 74 dB
ISO Shrinkage - Pressure 60 MPa