LATI Latiohm 36/07 PD01 G/20 ABS, 20% Glass Fiber Reinforced

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
Manufacturer LATI
Trade Name Latiohm
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latiohm 36/07 PD01 G/20 ABS, 20% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Semiconductive/dissipative product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
Linear Mold Shrinkage, Flow 0.0030 - 0.0045 cm/cm
0.0030 - 0.0045 in/in
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.0 MPa
12300 psi
Elongation at Break 1.2 %
1.2 %
Tensile Modulus 12.2 GPa
1770 ksi
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
Vicat Softening Point 100 °C

@Load 5.00 kg
212 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Volume Resistivity 500000 ohm-cm
500000 ohm-cm
Surface Resistance 1e+05
1e+05
Processing Properties Metric English Comments
Melt Temperature 220 - 250 °C
428 - 482 °F
Mold Temperature 50.0 - 80.0 °C
122 - 176 °F
Drying Temperature 70.0 - 80.0 °C

@Time 10800 sec
158 - 176 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa
Users viewing this material also viewed the following: