Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LATI Latishield 36/AR-10A-V0E ABS, Steel Fiber Reinforced, Flame Retardant

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled
Manufacturer LATI
Trade Name Latishield
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latishield 36/AR-10A-V0E ABS, Steel Fiber Reinforced, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Information provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
Linear Mold Shrinkage, Flow 0.0060 - 0.0085 cm/cm
0.0060 - 0.0085 in/in
Linear Mold Shrinkage, Transverse 0.0070 - 0.0095 cm/cm
0.0070 - 0.0095 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
Elongation at Break 2.2 %
2.2 %
Tensile Modulus 2.70 GPa
392 ksi
Charpy Impact Unnotched 1.00 J/cm²
4.76 ft-lb/in²
Charpy Impact, Notched 0.250 J/cm²
1.19 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
Vicat Softening Point 85.0 °C

@Load 5.00 kg
185 °F

@Load 11.0 lb
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Electrical Properties Metric English Comments
Surface Resistance 10 ohm
10 ohm
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Descriptive Properties Value Comments
Electromagnetic reflection 95 dB
ISO Shrinkage - Pressure 60 MPa
Users viewing this material also viewed the following: