Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LATI Latishield 52/5-07A PP Homopolymer, Steel Fiber Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Stainless Fiber, EMI
Manufacturer LATI
Trade Name Latishield
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latishield 52/5-07A PP Homopolymer, Steel Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EMI shielding product based on Polypropylene homopolymer (PPh). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
Linear Mold Shrinkage, Flow 0.014 - 0.017 cm/cm
0.014 - 0.017 in/in
Linear Mold Shrinkage, Transverse 0.014 - 0.017 cm/cm
0.014 - 0.017 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
Elongation at Break 20 %
20 %
Elongation at Yield 8.0 %
8.0 %
Tensile Modulus 2.00 GPa
290 ksi
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
Vicat Softening Point 105 °C

@Load 5.00 kg
221 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Surface Resistance 100 ohm
100 ohm
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Drying Temperature 80.0 - 90.0 °C
176 - 194 °F
Descriptive Properties Value Comments
Electromagnetic reflection 86 dB
ISO Shrinkage - Pressure 60 MPa