Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical 65IH HIPS

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer LG Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical 65IH HIPS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High impact, Extrusion, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include refrigerator food trays, and disposable food containers
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 3.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D785
Tensile Strength, Yield 29.5 MPa
4280 psi
50 mm/min; ASTM D638
Elongation at Break 60 %
60 %
50 mm/min; ASTM D638
Flexural Yield Strength 47.1 MPa
6830 psi
15 mm/min; ASTM D790
Flexural Modulus 2.10 GPa
305 ksi
15 mm/min; ASTM D790
Izod Impact, Notched 0.930 J/cm

@Thickness 6.35 mm
1.74 ft-lb/in

@Thickness 0.250 in
ASTM D256
1.37 J/cm

@Thickness 3.17 mm
2.57 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C

@Thickness 12.7 mm
172 °F

@Thickness 0.500 in
Unannealed; ASTM D648
Vicat Softening Point 99.0 °C
210 °F
1000 g; ASTM D1525
Flammability, UL94 HB
HB
1/16 in
HB
HB
1/8 in
Flame Spread 30.0 mm/min

@Thickness 3.17 mm
1.18 in/min

@Thickness 0.125 in
FH3
Electrical Properties Metric English Comments
Comparative Tracking Index 400 - 600 V
400 - 600 V
UL Rating PLC 1 (400-600 volts)
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL Rating PLC 3 (15-30 sec)
High Amp Arc Ignition, HAI >= 120 arcs
>= 120 arcs
UL Rating PLC 0 (>120 arcs)
High Voltage Arc-Tracking Rate, HVTR <= 10.0 mm/min
<= 0.394 in/min
UL Rating PLC 0 (0-10 mm/min)