Material Notes:
Advantage: Super slump retention; Low concrete viscosity; Good combination with water reducer (WRM, WB, RS)Main Uses: Super slump retentionInformation provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.06 - 1.10 g/cc
1.06 - 1.10 g/cc
Solids Content 39 - 41 %
39 - 41 %
pH 5.0 - 7.0
5.0 - 7.0
Viscosity 180 - 260 cP
180 - 260 cP
Descriptive Properties Value Comments
Chloride content >0.01%
Dosage 20% based 0.6-2.0%