Material Notes:
Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modifiers - Butadien type, Acryl type.Application: PC Alloy (PC, PC/ABS, PC/PBT) etcInformation provided by LG Chemical
Physical Properties Metric English Comments
Bulk Density >= 0.250 g/cc
>= 0.00903 lb/in³
Aerated; LSY-QB-KD019
Volatiles <= 1.0 %
<= 1.0 %
ISO 1625
Particle Mesh Size 20 Mesh
20 Mesh
<3%, (mesh on); LSY-QB-KD034
200 Mesh
200 Mesh
<35%, (mesh pass); LSY-QB-KD035
Mechanical Properties Metric English Comments
Izod Impact, Unnotched >= 0.981 J/cm

@Thickness 6.35 mm,
Temperature -30.0 °C
>= 1.84 ft-lb/in

@Thickness 0.250 in,
Temperature -22.0 °F
ISO 180
>= 3.92 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
>= 7.35 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ISO 180
>= 4.90 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
>= 9.18 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ISO 180
>= 5.88 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
>= 11.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ISO 180
Descriptive Properties Value Comments
Foreign Material <3 (10 x 10 cm)
LSY-QB-KD005
Fusion time <90 sec
ISO 1830-6