Excellent Barrier Performance, High StiffnessApplication:
Physical Properties Metric English Comments
Specific Gravity 0.954 g/cc
0.954 g/cc
Thermal Properties Metric English Comments
Melting Point 220 - 230 °C
428 - 446 °F