Material Notes:
Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7 and 14807-96-6Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D792
Melt Flow 40 g/10 min

@Load 10.0 kg,
Temperature 230 °C
40 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 72 - 78
72 - 78
ASTM D2240
Tensile Strength at Break 4.41 MPa

@Thickness 2.00 mm
640 psi

@Thickness 0.0787 in
50mm/min; ASTM D638
Elongation at Break 300 %

@Thickness 2.00 mm
300 %

@Thickness 0.0787 in
50mm/min; ASTM D638
Izod Impact, Notched NB

@Thickness 6.40 mm,
Temperature 23.0 °C
NB

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
NB

@Thickness 6.40 mm,
Temperature -40.0 °C
NB

@Thickness 0.252 in,
Temperature -40.0 °F
ASTM D256
Tear Strength 29.4 kN/m
168 pli
50mm/min, @ Break; ASTM D624
Processing Properties Metric English Comments
Rear Barrel Temperature 180 - 200 °C
356 - 392 °F
Injection Molding
Middle Barrel Temperature 180 - 220 °C
356 - 428 °F
Injection Molding
Front Barrel Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
Nozzle Temperature 200 - 240 °C
392 - 464 °F
Injection Molding
Melt Temperature 200 - 240 °C
392 - 464 °F
Injection Molding
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Injection Molding
Drying Temperature 60.0 - 90.0 °C
140 - 194 °F
Injection Molding
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Injection Molding
Back Pressure 29.4 - 58.8 MPa
4260 - 8530 psi
Injection Molding
Screw Speed 30 - 60 rpm
30 - 60 rpm
Injection Molding