Material Notes:
Features: Excellent toughness with flexible performance, High clarity and low temperature sealability. High performance in footwear applicationApplication: Polymer modification, Shoe sole, Film coextrusionCSA No. 26221-73-8Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.903 g/cc
0.903 g/cc
ASTM D1505
Mooney Viscosity 23

@Temperature 121 °C
23

@Temperature 250 °F
1+4(121); ASTM D1646
Melt Flow 1.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
ASTM D2240
Tensile Strength at Break 24.5 MPa
3550 psi
ASTM D638
Elongation at Break 660 %
660 %
ASTM D638
1% Secant Modulus 83.0 MPa
12000 psi
ASTM D790
Tear Strength 87.0 kN/m
497 pli
Type C; ASTM D624
Thermal Properties Metric English Comments
Melting Point 96.0 °C
205 °F
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746
Glass Transition Temp, Tg -31.0 °C
-23.8 °F