LG Chemical LUPOS HR-2307 Heat Resistant SAN, 30% Glass Fiber Reinforced

Category Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Molded, Glass Reinforced
Manufacturer LG Chemical
Trade Name LUPOS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical LUPOS HR-2307 Heat Resistant SAN, 30% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have a wide range of applications in automotive parts, electrical/electronic parts. and industrial equipments, etc.Applications: Automotive: Main core, glove box, meter box, head lamp housing, back mirror cover, etc.Electrical and Electronic: Computer tape reel, pan cake hub for video and audio, stereo speaker box, fan for air conditioner, washing machine pulley, fax frameOthers:Camera body, fishing reel, bobbinInformation Provided by LG Chem
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 127 MPa
18400 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 155 MPa
22500 psi
ASTM D790
Flexural Modulus 9.02 GPa
1310 ksi
ASTM D790
Izod Impact, Notched 0.390 J/cm

@Temperature 23.0 °C
0.731 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 108 °C
226 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Processing Properties Metric English Comments
Rear Barrel Temperature 210 - 230 °C
410 - 446 °F
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Front Barrel Temperature 230 - 250 °C
446 - 482 °F
Nozzle Temperature 230 - 250 °C
446 - 482 °F
Melt Temperature 240 - 260 °C
464 - 500 °F
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
Drying Temperature 90.0 °C
194 °F
Dry Time 3 - 4 hour
3 - 4 hour
Injection Pressure 78.45 - 88.26 MPa
11380 - 12800 psi
Second
68.65 - 98.07 MPa
9957 - 14220 psi
First
Back Pressure 0.000 - 3.92 MPa
0.000 - 569 psi
Screw Speed 40 - 60 rpm
40 - 60 rpm