LG Chemical LUPOY HR-5006A Heat Resistant PC/ABS Alloy, Unreinforced, Weather Resistant

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer LG Chemical
Trade Name LUPOY
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical LUPOY HR-5006A Heat Resistant PC/ABS Alloy, Unreinforced, Weather Resistant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive front ends, cluster pad main panel (instrument panel), lower cluster pad main, console box, glove box cover, door, wheel cover and cap, defroster grill, back mirror housingElectrical and Electronic: Monitor housing, fax housing, notebook PC housing, cellular phone case, fax and copy machine frame, CD ROM drive tray and main frame, relay case, connector, switchIndustrial Parts and Household Appliance: Helmet, terminal box, electrical tool housing, industrial bobbin, distributing board box, power tool component, gears and cams, water meter housingInformation Provided by LG Chem
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ASTM D955
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 250 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 482 °F
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Yield 55.0 MPa
7980 psi
ASTM D638
Elongation at Break >= 100 %
>= 100 %
ASTM D638
Flexural Strength 77.0 MPa
11200 psi
ASTM D790
Flexural Modulus 2.205 GPa
319.8 ksi
ASTM D790
Izod Impact, Notched 5.39 J/cm

@Temperature -30.0 °C
10.1 ft-lb/in

@Temperature -22.0 °F
ASTM D256
6.35 J/cm

@Temperature 23.0 °C
11.9 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 108 °C
226 °F
ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 220 - 260 °C
428 - 500 °F
Middle Barrel Temperature 230 - 270 °C
446 - 518 °F
Front Barrel Temperature 240 - 280 °C
464 - 536 °F
Nozzle Temperature 240 - 280 °C
464 - 536 °F
Melt Temperature 250 - 290 °C
482 - 554 °F
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
Drying Temperature 70.0 - 100 °C
158 - 212 °F
Dry Time 3 - 5 hour
3 - 5 hour
Screw Speed 40 - 70 rpm
40 - 70 rpm