LG Chemical LUTENE-H ME8000 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer LG Chemical
Trade Name LUTENE-H
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical LUTENE-H ME8000 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: LUTENE-H ME8000 is mainly intended for injection molding of containers. It has good mechanical properties and high productivity.Applications: Silicone cartridge, containers, complicated parts, toysCAS No. 9002-88-4Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.957 g/cc
0.957 g/cc
ASTM D1505
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 28.4 MPa
4120 psi
ASTM D638
Elongation at Break >= 1000 %
>= 1000 %
ASTM D638
Flexural Modulus 1.03 GPa
149 ksi
ASTM D790
Izod Impact, Notched 0.588 J/cm

@Temperature 23.0 °C
1.10 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Crystallization Temperature 134 °C
273 °F
Melting; DSC
Vicat Softening Point 125 °C
257 °F
ASTM D1525
Shrinkage 1.5 - 5.0 %
1.5 - 5.0 %
Depending on the processing conditions
Processing Properties Metric English Comments
Melt Temperature 220 - 260 °C
428 - 500 °F
Resin, Injection Molding
Mold Temperature 10.0 - 60.0 °C
50.0 - 140 °F
Injection Molding
Back Pressure 0.500 - 15.0 MPa
72.5 - 2180 psi
Injection Molding