LG Chemical LUTENE MB9205 LDPE Injection Molding Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer LG Chemical
Trade Name LUTENE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical LUTENE MB9205 LDPE Injection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: The physical and structural characteristics of LUTENE MB9205 give it excellent flow properties and good productivity, clarity and surface gloss.Main Application: Lids of all sizes, household articles, powder coatingCAS No. 9002-88-4Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.916 g/cc
0.916 g/cc
ASTM D1505
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 190 °C
24 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
ASTM D2240
Tensile Strength at Break 13.0 MPa
1890 psi
ASTM D638
Tensile Strength, Yield 9.32 MPa
1350 psi
ASTM D638
Elongation at Break 510 %
510 %
ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 81.0 °C
178 °F
ASTM D1525