LG Chemical PE1311 PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer LG Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical PE1311 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General Description: PE1311, homopolymer made by emulsion polymerization, is a high-viscosity PVC resin with pseudo-plastic flow property PE1311 has an good chemical foaming with low density and fine cell. Main Applications: Dipping, Low density foam layer in wall coverings and flooring, Synthetic leather Automotive underbody coater, High foaming productsCAS No: 9002-86-2Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.406 g/cc
1.406 g/cc
Bulk Density 0.310 - 0.410 g/cc
0.0112 - 0.0148 lb/in³
ASTM D1895
Volatiles <= 0.30 %

@Temperature 110 °C,
Time 3600 sec
<= 0.30 %

@Temperature 230 °F,
Time 1.00 hour
ASTM D3030-90
Brookfield Viscosity 10000 - 60000 cP
10000 - 60000 cP
DOP 60phr, 6RPM; ASTM D1824
Viscosity Measurement >= 5.0

@Pressure 0.400 MPa
>= 5.0

@Pressure 58.0 psi
[g/sec], DOP 60phr, Severs; ASTM D1823
Molecular Weight 60000 - 150000 g/mol
60000 - 150000 g/mol
Thermal Properties Metric English Comments
Melting Point 302 °C
576 °F
Descriptive Properties Value Comments
Autoignition Temperature 435°C
Degree of Polymerization 1200-1300
30°C, JIS K 6720-2
K-Value 70
DIN53726 / ISO1628-2