Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical Phenol

Category Fluid
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical Phenol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Structure & Characteristics: C6H5OH. Phenol is a white crystalline solid with a distinct smellUses: Raw material of phenolic resins, dye stuffs, synthetic fibers, herbicides, photo material, aromatic essences, etc. Moreover, it is also used as disinfectants and sterilizers. We also use phenol as the base material for our BPACAS: 108-95-2Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity >= 1.0009 g/cc
>= 1.0009 g/cc
1% aq' sol
Viscosity 1.09 cP

@Temperature 100 °C
1.09 cP

@Temperature 212 °F
1.56 cP

@Temperature 80.0 °C
1.56 cP

@Temperature 176 °F
2.47 cP

@Temperature 60.0 °C
2.47 cP

@Temperature 140 °F
3.8 cP

@Temperature 45.0 °C
3.8 cP

@Temperature 113 °F
Molecular Weight 94.11 g/mol
94.11 g/mol
Vapor Pressure 0.000280 bar

@Temperature 25.0 °C
0.210 torr

@Temperature 77.0 °F
0.00349 bar

@Temperature 50.0 °C
2.62 torr

@Temperature 122 °F
0.0540 bar

@Temperature 100 °C
40.5 torr

@Temperature 212 °F
0.52999 bar

@Temperature 160 °C
397.53 torr

@Temperature 320 °F
Thermal Properties Metric English Comments
Heat of Fusion 122.3 J/g
52.59 BTU/lb
Heat of Vaporization 489 J/g
210 BTU/lb
@ B.P.
Specific Heat Capacity 1.28 J/g-°C
0.306 BTU/lb-°F
Melting Point 37.9 °C
100 °F
Boiling Point 181.8 °C
359.2 °F
Flash Point 79.0 °C
174 °F
CC
85.0 °C
185 °F
TOC
Chemical Properties Metric English Comments
Critical Temperature 419 °C
786 °F
Descriptive Properties Value Comments
Autoignition Temperature 716°C
Color <10 Pt/Co
Molten
Clear
Components Water Content
<300 ppm
Explosion limit 0.015
Heat of Combustion -7.754 cal/g
Ignition Point >715°C
Purity >99.95%
Solidification >40.8°C
Copyright © lookpolymers.com All Rights Reserved