LG Chemical SEETEC BC500 LDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Wire/Cable Grade
Manufacturer LG Chemical
Trade Name SEETEC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical SEETEC BC500 LDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good Processability and Good electrical properties. Main Application: Cable insulationCAS No. 9002-88-4Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.918 - 0.922 g/cc
0.918 - 0.922 g/cc
ASTM D1505
Melt Flow 2.7 - 3.3 g/10 min

@Load 2.61 kg,
Temperature 190 °C
2.7 - 3.3 g/10 min

@Load 5.75 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 12.3 MPa
1780 psi
500mm/min; ASTM D638
Elongation at Break 600 %
600 %
500 mm/min; ASTM D638
2% Secant Modulus 1.20 GPa
174 ksi
500mm/min; ASTM D638
Thermal Properties Metric English Comments
Melting Point 105 °C
221 °F
10°C/min; ASTM D3418
150 - 200 °C
302 - 392 °F
Vicat Softening Point 90.0 °C
194 °F
ASTM D1525
Electrical Properties Metric English Comments
Dielectric Constant 2.28
2.28
ASTM D1531