LG Chemical SEETEC EF221 Ethylene Vinyl Acetate

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Manufacturer LG Chemical
Trade Name SEETEC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical SEETEC EF221 Ethylene Vinyl Acetate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: Good Mechanical Properties and Good Optical Properties Additives: Antiblocking agent, Slip AgentApplications: Agricultural FilmCAS No. 24937-78-8Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.924 - 0.928 g/cc
0.924 - 0.928 g/cc
ASTM D1505
Melt Flow 0.50 - 0.70 g/10 min

@Load 2.61 kg,
Temperature 190 °C
0.50 - 0.70 g/10 min

@Load 5.75 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 17.7 MPa
2560 psi
500mm/min; ASTM D638
Film Elongation at Break, MD 400 %
400 %
500 mm/min; ASTM D638
Film Elongation at Break, TD 650 %
650 %
500 mm/min; ASTM D638
Elongation at Break 700 %
700 %
500 mm/min; ASTM D638
2% Secant Modulus 1.05 GPa
152 ksi
500mm/min; ASTM D638
Elmendorf Tear Strength MD 350 g
350 g
ASTM D1922
Elmendorf Tear Strength TD 250 g
250 g
ASTM D1922
Dart Drop Test 250 g
0.551 lb
ASTM D1709
Film Tensile Strength at Break, MD 31.4 MPa
4550 psi
500mm/min, Ultimate; ASTM D638
Film Tensile Strength at Break, TD 29.4 MPa
4260 psi
500mm/min, Ultimate; ASTM D638
Thermal Properties Metric English Comments
Melting Point 103 °C
217 °F
10°C/min; ASTM D3418
Vicat Softening Point 94.0 °C
201 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
ASTM D1003
Gloss 95 %
95 %
45°; ASTM D2457