LG Chemical SEETEC PM360 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer LG Chemical
Trade Name SEETEC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical SEETEC PM360 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Characteristics: Excellent processability, Good tenacity & knot strengthAdditives: Anti-oxidants, LubricantsApplication: Tarpaulin, Woven bags (Inflation)CAS No. 25213-02-9Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.949 - 0.952 g/cc
0.949 - 0.952 g/cc
ASTM D1505
Melt Flow 0.70 - 0.85 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 - 0.85 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 50
50
ASTM D785
Tensile Strength at Break 28.0 MPa
4060 psi
50mm/min; ASTM D638
Tensile Strength, Yield 24.5 MPa
3560 psi
50 mm/min; ASTM D638
Elongation at Break >= 500 %

@Thickness 50.0 mm
>= 500 %

@Thickness 1.97 in
ASTM D638
Flexural Modulus 1.27 GPa
185 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 131 °C
268 °F
10°C/min; ASTM D3418
Vicat Softening Point 124 °C
255 °F
ASTM D1525