Material Notes:
Forms: PelletsInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Water Absorption 0.26 %
0.26 %
at 24 hrs; ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0050 in/in

@Thickness 0.126 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 128 MPa
18600 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 186 MPa
27000 psi
ASTM D790
Flexural Modulus 5.88 GPa
853 ksi
ASTM D790
Izod Impact, Notched 0.490 J/cm
0.918 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 35.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
19.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 210 °C

@Thickness 3.20 mm
410 °F

@Thickness 0.126 in
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 1.00e+6 - 1.00e+8 ohm
1.00e+6 - 1.00e+8 ohm
ASTM D257
Users viewing this material also viewed the following: