LTL Color Compounds ColorFast® PCT1000 PC/PET Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer LTL Color Compounds
Trade Name ColorFast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LTL Color Compounds ColorFast® PCT1000 PC/PET Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PC/PET alloy with outstanding chemical resistance and impact strengthAll information provided by LTL Color Compounders, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Melt Flow 18 g/10 min

@Load 3.80 kg,
Temperature 260 °C
18 g/10 min

@Load 8.38 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.7 MPa
7500 psi
2.0 in/min; ASTM D638
Flexural Strength 75.8 MPa
11000 psi
2.0 in/min; ASTM D790
Flexural Modulus 1.93 GPa
280 ksi
2.0 in/min; ASTM D790
Izod Impact, Notched 6.94 J/cm

@Temperature 22.8 °C
13.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256