Material Notes:
A biocompatible, high gloss injection molding grade of ABS for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided by LTL Color Compounders, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Melt Flow 5.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 47.6 MPa
6900 psi
ASTM D638
Elongation at Break 26 %
26 %
ASTM D638
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Notched 2.14 J/cm

@Temperature 22.8 °C
4.00 ft-lb/in

@Temperature 73.0 °F
0.125"; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 83.9 °C
183 °F
Unannealed (0.5"); ASTM D648