Material Notes:
DYNAFLEX VAC-ARC steel is a medium alloyed, air hardening ultra high strength grade designed for structural applications requiring room temperature tensile strengths of 220,000 to 300,000 psi. Due to the secondary hardening feature exhibited by this alloy, stable elevated temperature properties are available up to Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Density 7.81 g/cc
0.282 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1790 MPa
260000 psi
Tensile Strength, Yield 1585 MPa

@Strain 0.200 %
229900 psi

@Strain 0.200 %
<150 in<sup>2</sup>
Reduction of Area 6.0 %
6.0 %
Modulus of Elasticity 207 GPa
30000 ksi
159 GPa

@Temperature 538 °C
23000 ksi

@Temperature 1000 °F
186 GPa

@Temperature 204 °C
27000 ksi

@Temperature 399 °F
Thermal Properties Metric English Comments
CTE, linear 11.5 µm/m-°C

@Temperature 21.0 - 204 °C
6.39 µin/in-°F

@Temperature 69.8 - 399 °F
13.1 µm/m-°C

@Temperature 21.0 - 648 °C
7.28 µin/in-°F

@Temperature 69.8 - 1200 °F
Specific Heat Capacity 0.460 J/g-°C

@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F

@Temperature 32.0 - 212 °F
Component Elements Properties Metric English Comments
Carbon, C 0.40 %
0.40 %
Chromium, Cr 5.0 %
5.0 %
Iron, Fe 91.6 %
91.6 %
Manganese, Mn 0.30 %
0.30 %
Molybdenum, Mo 1.3 %
1.3 %
Silicon, Si 0.90 %
0.90 %
Vanadium, V 0.50 %
0.50 %
Chemical Properties Metric English Comments
Critical Temperature 815 °C
1500 °F