Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Latrobe LSSâ„¢ 2367 Hot Work Tool Steel

Category Metal , Ferrous Metal , Alloy Steel , Chrome-moly Steel , Tool Steel , Hot Work Steel
Manufacturer Latrobe Steel
Trade Name LSS™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe LSSâ„¢ 2367 Hot Work Tool Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TLS 2367 is a chromium-molybdenum hot work steel that is similar to AISI H11 hot work steel, but which contains a higher molybdenum content. The higher molybdenum gives TLS 2367 better hot hardness and temper resistance, along with higher attainable hardness and deeper hardenability than the more common H11 and H13 hot work steels. Typical applications include extrusion tooling, hot forging dies, hot heading dies, hot shear blades, hot punches and mandrels, hot gripper dies, and die casting tooling for copper and brass.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Mechanical Properties Metric English Comments
Hardness, Rockwell C 56
56
Oil Quenched from 1024°C, 45 minutes
57
57
Oil Quenched from 1080°C, 20 minutes
Machinability 75 - 80 %
75 - 80 %
1% Carbon Steel
Thermal Properties Metric English Comments
CTE, linear 11.9 µm/m-°C

@Temperature 20.0 - 100 °C
6.61 µin/in-°F

@Temperature 68.0 - 212 °F
13.1 µm/m-°C

@Temperature 20.0 - 500 °C
7.28 µin/in-°F

@Temperature 68.0 - 932 °F
Thermal Conductivity 27.5 W/m-K

@Temperature 700 °C
191 BTU-in/hr-ft²-°F

@Temperature 1290 °F
32.2 W/m-K

@Temperature 350 °C
223 BTU-in/hr-ft²-°F

@Temperature 662 °F
36.4 W/m-K

@Temperature 20.0 °C
253 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Component Elements Properties Metric English Comments
Carbon, C 0.38 %
0.38 %
Chromium, Cr 5.0 %
5.0 %
Iron, Fe 90.22 %
90.22 %
Manganese, Mn 0.45 %
0.45 %
Molybdenum, Mo 3.0 %
3.0 %
Silicon, Si 0.40 %
0.40 %
Vanadium, V 0.55 %
0.55 %
Chemical Properties Metric English Comments
Critical Temperature 850 °C
1560 °F
Ae1
853 °C
1570 °F
Ar1
Users viewing this material also viewed the following: