Material Notes:
TLS 2714 is a nickel-chromium-molybdenum hot work steel that exhibits high impact toughness and good resistance to softening at elevated temperature. The high nickel content imparts the toughness as well as good through-hardening (hardenability) in large section thicknesses. The steel also exhibits good resistance to thermal shock and thermal fatigue cracking, and relatively small dimensional changes during hardening.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Mechanical Properties Metric English Comments
Hardness, Rockwell C 53
53
Air Cooled from 860°C, 45 minutes
55
55
Oil Quenched from 830°C, 45 minutes
57
57
Air Cooled from 900°C, 45 minutes
59
59
Oil Quenched from 870°C, 45 minutes
Machinability 75 - 80 %
75 - 80 %
1% Carbon Steel
Thermal Properties Metric English Comments
CTE, linear 12.2 µm/m-°C

@Temperature 20.0 - 100 °C
6.78 µin/in-°F

@Temperature 68.0 - 212 °F
14.2 µm/m-°C

@Temperature 20.0 - 500 °C
7.89 µin/in-°F

@Temperature 68.0 - 932 °F
Thermal Conductivity 35.0 W/m-K

@Temperature 700 °C
243 BTU-in/hr-ft²-°F

@Temperature 1290 °F
36.0 W/m-K

@Temperature 20.0 °C
250 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
38.0 W/m-K

@Temperature 350 °C
264 BTU-in/hr-ft²-°F

@Temperature 662 °F
Component Elements Properties Metric English Comments
Carbon, C 0.50 %
0.50 %
Chromium, Cr 1.3 %
1.3 %
Iron, Fe 94.85 %
94.85 %
Manganese, Mn 0.85 %
0.85 %
Molybdenum, Mo 0.50 %
0.50 %
Nickel, Ni 1.65 %
1.65 %
Silicon, Si 0.25 %
0.25 %
Vanadium, V 0.10 %
0.10 %
Chemical Properties Metric English Comments
Critical Temperature 732 °C
1350 °F
Ac1
771 °C
1420 °F
Ac3