Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lavergne VYPET VNT 1020 Polyester-PC Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Lavergne Performance Compounds
Trade Name VYPET
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lavergne VYPET VNT 1020 Polyester-PC Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Vypet 1020 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemical ResistanceTypical Applications: Automotive; IndustrialInformation provided by Bieglo Gmbh for Lavergne Performance Compounds
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0080 - 0.010 cm/cm
0.0080 - 0.010 in/in
3.2 mm; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
5 mm/min; ASTM D638
Flexural Strength 70.0 MPa
10200 psi
1.3 mm/min; ASTM D790
Flexural Modulus 2.10 GPa
305 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 5.20 J/cm

@Temperature 23.0 °C
9.74 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
ASTM D648
Processing Properties Metric English Comments
Feed Temperature 245 - 255 °C
473 - 491 °F
Middle Barrel Temperature 250 - 260 °C
482 - 500 °F
Front Barrel Temperature 255 - 265 °C
491 - 509 °F
Nozzle Temperature 260 - 270 °C
500 - 518 °F
Melt Temperature 260 - 275 °C
500 - 527 °F
Mold Temperature 18.0 - 75.0 °C
64.4 - 167 °F
Injection Pressure 69.0 - 138 MPa
10000 - 20000 psi
Copyright © lookpolymers.com All Rights Reserved