Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 1-8490 Polyamide 66, with carbon fiber, heat stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Carbon Fiber Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1-8490 Polyamide 66, with carbon fiber, heat stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stable precision parts with low warpage and narrow tolerance range.Gear parts for automotive appliances, control disks, cams, sliding elements.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ISO 1183
Water Absorption <= 1.0 %
<= 1.0 %
23°C/24h
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Stress 140 MPa
20300 psi
Elongation at Yield 1.5 %
1.5 %
2.0 %
2.0 %
flexural
Modulus of Elasticity 18.0 GPa
2610 ksi
Flexural Strength 200 MPa
29000 psi
Flexural Modulus 15.0 GPa
2180 ksi
Charpy Impact Unnotched 2.20 J/cm²
10.5 ft-lb/in²
edgewise; ISO 179 1eU
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
160 °C
320 °F
short term
Electrical Properties Metric English Comments
Surface Resistance <= 1.00e+12 ohm
<= 1.00e+12 ohm
Insulation Resistance <= 1.00e+12 ohm
<= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 290 °C
554 °F
mass temp
Nozzle Temperature 280 - 300 °C
536 - 572 °F
Zone 1 290 - 310 °C
554 - 590 °F
Zone 2 290 - 310 °C
554 - 590 °F
Zone 3 290 - 310 °C
554 - 590 °F
Mold Temperature 90.0 - 120 °C
194 - 248 °F
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
105 °C

@Time 14400 - 21600 sec
221 °F

@Time 4.00 - 6.00 hour
Vacuum Dryer
Descriptive Properties Value Comments
Color natural color (black)
Users viewing this material also viewed the following: