Lehmann & Voss LUVOCOM® 1100-8301 Polyether sulfone, with carbon fiber, PTFE, lubricant modified

Category Polymer , Thermoplastic , Polyethersulfone (PES) , Polyethersulfone, Carbon Fiber Reinforced
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1100-8301 Polyether sulfone, with carbon fiber, PTFE, lubricant modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Low warpage.Improved friction and wear behaviour. Emergency running property.Bearings, sleeves, control disks, gear wheels, pump impellers, gear parts.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.51 g/cc
1.51 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
23°C/24h
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
Melt Flow 12.08 g/10 min

@Load 5.00 kg,
Temperature 345 °C
12.08 g/10 min

@Load 11.0 lb,
Temperature 653 °F
Mechanical Properties Metric English Comments
Tensile Stress 90.0 MPa
13100 psi
Elongation at Yield 2.0 %
2.0 %
2.7 %
2.7 %
flexural
Modulus of Elasticity 10.0 GPa
1450 ksi
Flexural Strength 125 MPa
18100 psi
Flexural Modulus 8.00 GPa
1160 ksi
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
edgewise; ISO 179 1eU
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179 1eA
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
200 °C
392 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
Electrical Properties Metric English Comments
Surface Resistance <= 1.00e+6 ohm
<= 1.00e+6 ohm
Insulation Resistance <= 1.00e+6 ohm
<= 1.00e+6 ohm
Processing Properties Metric English Comments
Processing Temperature 350 °C
662 °F
mass temp
Nozzle Temperature 340 - 360 °C
644 - 680 °F
Zone 1 355 - 375 °C
671 - 707 °F
Zone 2 360 - 380 °C
680 - 716 °F
Zone 3 350 - 370 °C
662 - 698 °F
Mold Temperature 120 - 200 °C
248 - 392 °F
Drying Temperature 150 °C

@Time 10800 - 18000 sec
302 °F

@Time 3.00 - 5.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color natural color (black)