Lehmann & Voss LUVOCOM® 1105-7107/BK PEEK, with glass fiber, easy flowing

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Glass Fiber Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1105-7107/BK PEEK, with glass fiber, easy flowing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
23°C/24h
Linear Mold Shrinkage 0.0050 - 0.010 cm/cm
0.0050 - 0.010 in/in
Melt Flow 58 g/10 min

@Load 10.0 kg,
Temperature 380 °C
58 g/10 min

@Load 22.0 lb,
Temperature 716 °F
Mechanical Properties Metric English Comments
Tensile Stress 115 MPa
16700 psi
Elongation at Yield 2.0 %
2.0 %
2.5 %
2.5 %
flexural
Modulus of Elasticity 7.00 GPa
1020 ksi
Flexural Strength 150 MPa
21800 psi
Flexural Modulus 6.50 GPa
943 ksi
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
flatwise; ISO 179 1fU
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179 1eA
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C
16.7 µin/in-°F
DIN 53752
Maximum Service Temperature, Air 250 °C
482 °F
260 °C
500 °F
short term
Flammability, UL94 V-0
V-0
not recognized by UL
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
Insulation Resistance >= 1.00e+16 ohm
>= 1.00e+16 ohm
Processing Properties Metric English Comments
Processing Temperature 390 °C
734 °F
mass temp
Nozzle Temperature 360 - 380 °C
680 - 716 °F
Zone 1 360 - 370 °C
680 - 698 °F
Zone 2 380 - 390 °C
716 - 734 °F
Zone 3 390 - 400 °C
734 - 752 °F
Mold Temperature 170 - 200 °C
338 - 392 °F
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
150 °C

@Time 10800 - 21600 sec
302 °F

@Time 3.00 - 6.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color black