Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 1105-7909/GY 2 PEEK, with carbon fiber

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1105-7909/GY 2 PEEK, with carbon fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flammable.Bearings, sleeves, control disks, gear wheels, pump impellers, gear parts.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
23°C/24h
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
Melt Flow 29.6 g/10 min

@Load 10.0 kg,
Temperature 380 °C
29.6 g/10 min

@Load 22.0 lb,
Temperature 716 °F
Mechanical Properties Metric English Comments
Tensile Stress 215 MPa
31200 psi
Elongation at Yield 2.0 %
2.0 %
2.5 %
2.5 %
flexural
Modulus of Elasticity 17.0 GPa
2470 ksi
Flexural Strength 310 MPa
45000 psi
Flexural Modulus 14.5 GPa
2100 ksi
Charpy Impact Unnotched 4.50 J/cm²
21.4 ft-lb/in²
edgewise; ISO 179 1eU
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179 1eA
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
280 °C
536 °F
short term
Flammability, UL94 V-0
V-0
not recognized by UL
Electrical Properties Metric English Comments
Surface Resistance <= 1.00e+6 ohm
<= 1.00e+6 ohm
Insulation Resistance <= 1.00e+6 ohm
<= 1.00e+6 ohm
Processing Properties Metric English Comments
Processing Temperature 390 °C
734 °F
mass temp
Nozzle Temperature 360 - 380 °C
680 - 716 °F
Zone 1 360 - 370 °C
680 - 698 °F
Zone 2 380 - 390 °C
716 - 734 °F
Zone 3 390 - 400 °C
734 - 752 °F
Mold Temperature 170 - 200 °C
338 - 392 °F
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
150 °C

@Time 10800 - 21600 sec
302 °F

@Time 3.00 - 6.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color grey
Users viewing this material also viewed the following: