Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5-1 PPS, linear, with carbon fiber and PTFE

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5-1 PPS, linear, with carbon fiber and PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous discharging of statically generated electricity.Suitable for metall inserts.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ISO 1183
Water Absorption <= 0.050 %
<= 0.050 %
23°C/24h
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm
0.0010 - 0.0040 in/in
Mechanical Properties Metric English Comments
Tensile Stress 140 MPa
20300 psi
Elongation at Yield 1.2 %
1.2 %
1.5 %
1.5 %
flexural
Modulus of Elasticity 15.0 GPa
2180 ksi
Flexural Strength 200 MPa
29000 psi
Flexural Modulus 13.0 GPa
1890 ksi
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
edgewise; ISO 179 1eU
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 220 °C
428 °F
240 °C
464 °F
short term
Electrical Properties Metric English Comments
Surface Resistance <= 10000 ohm
<= 10000 ohm
Insulation Resistance <= 1.00e+6 ohm
<= 1.00e+6 ohm
Processing Properties Metric English Comments
Processing Temperature 330 °C
626 °F
mass temp
Nozzle Temperature 320 - 340 °C
608 - 644 °F
Zone 1 300 - 320 °C
572 - 608 °F
Zone 2 310 - 330 °C
590 - 626 °F
Zone 3 320 - 340 °C
608 - 644 °F
Mold Temperature 150 - 180 °C
302 - 356 °F
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color black