Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15 PPS, linear, with glass fiber and PTFE

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15 PPS, linear, with glass fiber and PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts with low creep.Improved friction and wear behaviour. Emergency running property.High chemical resistance parts.Control disks, gear wheels, pump impellers, gear parts for automotive appliances, chip carrier.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.69 g/cc
1.69 g/cc
ISO 1183
Water Absorption <= 0.050 %
<= 0.050 %
23°C/24h
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
Mechanical Properties Metric English Comments
Tensile Stress 130 MPa
18900 psi
Elongation at Yield 2.0 %
2.0 %
3.0 %
3.0 %
flexural
Modulus of Elasticity 11.0 GPa
1600 ksi
Flexural Strength 200 MPa
29000 psi
Flexural Modulus 10.0 GPa
1450 ksi
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
flatwise; ISO 179 1fU
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179 1eA
Coefficient of Friction, Dynamic 0.20
0.20
Coefficient of Friction, Static 0.15
0.15
Thermal Properties Metric English Comments
CTE, linear 25.0 µm/m-°C
13.9 µin/in-°F
DIN 53752
Thermal Conductivity 0.400 W/m-K
2.78 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 220 °C
428 °F
240 °C
464 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
Vicat Softening Point 240 °C
464 °F
DIN ISO 306
Flammability, UL94 V-0
V-0
not recognized by UL
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 330 °C
626 °F
mass temp
Nozzle Temperature 320 - 340 °C
608 - 644 °F
Zone 1 300 - 320 °C
572 - 608 °F
Zone 2 310 - 330 °C
590 - 626 °F
Zone 3 320 - 340 °C
608 - 644 °F
Mold Temperature 150 - 180 °C
302 - 356 °F
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color natural color (beige)