Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 3-7837 Polyamide 6, unreinforced, thermally conductive modified

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 3-7837 Polyamide 6, unreinforced, thermally conductive modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.Isotropic shrinkage characteristics.Reduced moment of inertia compared with metal parts.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.89 g/cc
1.89 g/cc
ISO 1183
Water Absorption <= 1.3 %
<= 1.3 %
23°C/24h
Linear Mold Shrinkage 0.0080 - 0.010 cm/cm
0.0080 - 0.010 in/in
Melt Flow <= 15 g/10 min

@Load 10.0 kg,
Temperature 275 °C
<= 15 g/10 min

@Load 22.0 lb,
Temperature 527 °F
Mechanical Properties Metric English Comments
Tensile Stress 55.0 MPa
7980 psi
Elongation at Yield 1.8 %
1.8 %
2.2 %
2.2 %
flexural
Modulus of Elasticity 5.50 GPa
798 ksi
Flexural Strength 80.0 MPa
11600 psi
Flexural Modulus 4.50 GPa
653 ksi
Charpy Impact Unnotched 2.40 J/cm²
11.4 ft-lb/in²
edgewise; ISO 179 1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179 1eA
Thermal Properties Metric English Comments
Thermal Conductivity 3.00 W/m-K
20.8 BTU-in/hr-ft²-°F
HOT-DISK || 60x60x3 mm
Maximum Service Temperature, Air 90.0 °C
194 °F
130 °C
266 °F
short term
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 270 °C
518 °F
mass temp
Nozzle Temperature 270 - 280 °C
518 - 536 °F
Zone 1 250 - 270 °C
482 - 518 °F
Zone 2 270 - 290 °C
518 - 554 °F
Zone 3 280 - 300 °C
536 - 572 °F
Mold Temperature 70.0 - 110 °C
158 - 230 °F
Drying Temperature 75.0 °C

@Time 36000 - 57600 sec
167 °F

@Time 10.0 - 16.0 hour
Dehumidifying dryer
105 °C

@Time 14400 - 21600 sec
221 °F

@Time 4.00 - 6.00 hour
or
Descriptive Properties Value Comments
Color dark grey