Material Notes:
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ISO 1183
Water Absorption <= 0.30 %
<= 0.30 %
23°C/24h
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm
0.0030 - 0.0070 in/in
Mechanical Properties Metric English Comments
Tensile Stress 30.0 MPa
4350 psi
Elongation at Yield 2.0 %
2.0 %
2.6 %
2.6 %
flexural
Modulus of Elasticity 6.00 GPa
870 ksi
Flexural Strength 40.0 MPa
5800 psi
Flexural Modulus 5.00 GPa
725 ksi
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
edgewise; ISO 179 1eU
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
130 °C
266 °F
short term
Vicat Softening Point 80.0 °C
176 °F
DIN ISO 306
Electrical Properties Metric English Comments
Surface Resistance <= 100 ohm
<= 100 ohm
Insulation Resistance <= 100 ohm
<= 100 ohm
Processing Properties Metric English Comments
Processing Temperature 230 - 260 °C
446 - 500 °F
mass temp
Nozzle Temperature 220 - 250 °C
428 - 482 °F
Zone 1 220 - 250 °C
428 - 482 °F
Zone 2 220 - 250 °C
428 - 482 °F
Zone 3 230 - 260 °C
446 - 500 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Drying Temperature 70.0 - 95.0 °C

@Time 7200 - 14400 sec
158 - 203 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color black
Copyright © lookpolymers.com All Rights Reserved