Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOTECH® GS 46 Polyamide 46, lubricant modified, heat stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 46
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOTECH®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOTECH® GS 46 Polyamide 46, lubricant modified, heat stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Highly dimensionally stable at elevated temperatures.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ISO 1183
Water Absorption <= 1.5 %
<= 1.5 %
23°C/24h
Linear Mold Shrinkage 0.010 - 0.015 cm/cm
0.010 - 0.015 in/in
Mechanical Properties Metric English Comments
Tensile Stress 100 MPa
14500 psi
Elongation at Yield 5.0 %
5.0 %
Modulus of Elasticity 3.90 GPa
566 ksi
Charpy Impact Unnotched 9.00 J/cm²
42.8 ft-lb/in²
flatwise; ISO 179 1fU
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179 1eA
Coefficient of Friction, Dynamic 0.31
0.31
Coefficient of Friction, Static 0.23
0.23
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
160 °C
320 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Vicat Softening Point 280 °C
536 °F
DIN ISO 306
Processing Properties Metric English Comments
Processing Temperature 310 °C
590 °F
mass temp
Nozzle Temperature 280 - 330 °C
536 - 626 °F
Zone 1 285 - 315 °C
545 - 599 °F
Zone 2 305 - 315 °C
581 - 599 °F
Zone 3 305 - 315 °C
581 - 599 °F
Mold Temperature 120 - 140 °C
248 - 284 °F
Drying Temperature 80.0 °C

@Time 7200 - 43200 sec
176 °F

@Time 2.00 - 12.0 hour
Vacuum Dryer
80.0 °C

@Time 7200 - 28800 sec
176 °F

@Time 2.00 - 8.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color umbra grey