Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Bearings, sleeves, sliding elements, control disks, gear wheels, duty parts in switches.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ISO 1183
Water Absorption <= 1.0 %
<= 1.0 %
23°C/24h
Linear Mold Shrinkage 0.015 - 0.025 cm/cm
0.015 - 0.025 in/in
Mechanical Properties Metric English Comments
Tensile Stress 65.0 MPa
9430 psi
Elongation at Yield 6.0 %
6.0 %
Modulus of Elasticity 2.80 GPa
406 ksi
Charpy Impact Unnotched 4.50 J/cm²
21.4 ft-lb/in²
flatwise; ISO 179 1fU
4.00 J/cm²

@Temperature -30.0 °C
19.0 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Coefficient of Friction, Dynamic 0.19
0.19
Coefficient of Friction, Static 0.13
0.13
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
140 °C
284 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
Vicat Softening Point 240 °C
464 °F
DIN ISO 306
Processing Properties Metric English Comments
Processing Temperature 290 °C
554 °F
mass temp
Nozzle Temperature 280 - 300 °C
536 - 572 °F
Zone 1 290 - 310 °C
554 - 590 °F
Zone 2 290 - 310 °C
554 - 590 °F
Zone 3 290 - 310 °C
554 - 590 °F
Mold Temperature 90.0 - 120 °C
194 - 248 °F
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
105 °C

@Time 14400 - 21600 sec
221 °F

@Time 4.00 - 6.00 hour
Vacuum Dryer
Descriptive Properties Value Comments
Color black