Loctite® 7113 Heptane Base Accelerator

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Loctite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® 7113 Heptane Base Accelerator.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Surface PreparersLoctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the cure speed and gap filling capabilities of Cyanoacrylate Adhesives. Activators are specially engineered curing agents for Structural Adhesives. Loctite® Primers are used to ensure cure on inactive surfaces and speed the cure of machinery adhesives.All Loctite® Surface Preparation products are available in ozone-safe (non-CFC) solvent-based and solventless formulations.Loctite® 7113 Heptane Base AcceleratorThis accelerator features long on-part life. Use with all Loctite® Cyanoacrylate Adhesives. Typical Use: All cyanoacrylates
Physical Properties Metric English Comments
Viscosity 0.40 cP
0.40 cP
Processing Properties Metric English Comments
Cure Time 1.00 min
0.0167 hour
Dry Time
1440 min
24.0 hour
On-Part Life
Descriptive Properties Value Comments
Color Clear