Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loctite® Tak Pak® 444 Instant Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Loctite
Trade Name Tak Pak®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® Tak Pak® 444 Instant Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cyanoacrylate Bonding Adhesives and Gasketing and Wire TackersLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-specific, instant adhesives. Loctite® Instant Adhesives are available in a variety of viscosities, cure speeds, gap-filling capability and substrate compatibility. The ultra high-performance PRISM® family offers additional products that surpass the most stringent demands, including toughened formulations, low odor and low blooming products, surface insensitive and thermally resistant formulations.Loctite® innovative gasketing products offer precise, reliable sealing of electronic enclosures, protecting them from environmental hazards. Loctite offers both Form-in-place (FIP) and Cure-in-Place (CIP) compression gasket materials.Loctite® Tak Pak Adhesives are used to secure wires to printed circuit board assemblies. The fast cure times of these adhesives help increase the throughput of the wire tacking assembly process.Loctite® 444 General Purpose Ethyl Tak Pak™ Instant AdhesiveAn adhesive designed for printed circuit board assembly and repair. Cures instantly with Tak Pak® Accelerator. Used to tack jumper wires and wires to coil forms. Tamper-proof adjustable components. Mounting standoffs, edge guides and stiffeners to circuit boards. Cure Type: Accelerator Bonding Type: Ethyl cyanoacrylate Commercial item std. A-A-3097 Type II, Class 3 Typical Use: Tak Pak® Wire tacking adhesive
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Viscosity 700 cP
700 cP
Mechanical Properties Metric English Comments
Adhesive Bond Strength 22.1 MPa
3200 psi
Grit blasted steel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.2 °C
180 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 0.500 min
0.00833 hour
1440 min
24.0 hour
Full Cure; Varies with substrates
Descriptive Properties Value Comments
Color Clear
Gap Fill 0.007 in.
Copyright © lookpolymers.com All Rights Reserved